MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: DOW Polyethylene 5004I extrusion coating resin is a low melt index resin for heavy duty applications such as paperboard coatings, milk cartons and folding cartons, aseptic package coatings, bag liner coatings, paper foil laminations, and for many other heavy duty applications. LDPE 5004I has a melt index and density which optimize processing, coating integrity, heat sealability and adhesion. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.2 for food contact applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/cc
Melt Flow 4.0 g/10 min
@Load 2.16 kg
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 4005 Low Density Polyethylene, Extrusion Coating Grade
Dow LDPE 4012 Low Density Polyethylene, Extrusion Coating Grade
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade

PDW494 / 34563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.