Product Description: PPC08N-SHI is a high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics and improved cycle time. PPC08N-SHI has balanced stiffness/toughness, fast molding cycle, high impact resistance, high stiffness, medium flow and nucleated. Applications include; appliances, automotive applications, child safety seals, consumer and industrial applications and rigid packaging. Availability: North America Additive: Nucleating Agent Features: Fast Molding Cycle; Good Processability; High Impact Resistance; High Stiffness; High Toughness; Highly Crystalline; Impact Copolymer; Medium Flow; Nucleated Uses: Appliances; Automotive Applications; Consumer Applications; Industrial Applications; Packaging; Seals Processing Method: Injection Molding Information provided by Osterman & Company |