MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Colmant Coated Fabrics EPDM Coated Polyester Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: EPDM coated polyester fabric combines the following properties: EPDM rubber has very good resistance to weather, heat, cold, ozone, aging, acids, polar solvents (water, ketones, alcohols, glycols). Good dielectric strength. Low resistance to fuels, chlorinated, aromatic or aliphatic solvents, petroleum derivatives and oils. Low resistance to fire. Flame spread is low. Polyester is a synthetic fiber that ranks first in the world in terms of production. It is a linear polymer whose mass includes a majority (80% minimum) of ester functions and terephthalic acid. Polyester yarn is light and flexible. It is resistant to ultraviolet radiation. Polyester fabric is hardly inflammable. It softens around 245°C, and melts around 250°C. It retains a good shape memory and can therefore be used in the composition of crease-resistant fabrics. Moreover, an adequate weaving also allows a good evacuation of heat.

Applications:

  • Industrial fabrics
  • straps
  • tarps
  • tires
  • rope
  • clothing
  • windshields gaskets
  • molded or extruded products.
Properties:
  • Heat resistant
  • Fireproofed
  • Acids resistance
  • Non-skid
  • UV resistance
  • Water storage
  • Ozone Resistance
  • Isolation to radiation

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 9030 - 90
Tensile Strength at Break 8.00 - 20.0 MPa1160 - 2900 psi
Elongation at Break 100 - 900 %100 - 900 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-55 C° - 140°C
Warp breaking strength90 - 2000 daN/5cm
Warp elongation at break10% - 20%
Weft breaking strength80 - 1400 daN/5cm
Weft elongation at break10% - 20%
Weight per sqm90 - 1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLMANT082 / 316132

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.