MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nanocyl EPOCYL™ NC E1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for non-Solvent Formulation Purposes
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: EPOCYL™ NC E1MY-02 is a Mater Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enhance electrical conductivity of high Tg epoxy-based formulations. Special features include easy integration and great flexibility in processing. Dilution factor has to be calculated accordingly to the desired level of conductivity.

Applications

  • Electrostatic discharge (ESD) coatings, linings (tanks, rollers, ...) and composites
  • Conductive primers
  • Resistive inks
  • Adhesives

Benefits

  • Limited impact on base resin mechanical and thermo-mechanical properties
  • Ease of formulation
  • Other information available upon request to Nanocyl

Curing agents EPOCYL™ NCE1MY-02 based formulations can be cured or cross-linked with different types of curing agents which could be decided accordingly to the desired processing conditions and the properties of the final composite like any conventional tetrafunctional based formulations.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 - 1.18 g/cc1.15 - 1.18 g/cc
Viscosity  5000 - 35000 cP
@Temperature 60.0 °C
5000 - 35000 cP
@Temperature 140 °F
Measured with parallel plate in dynamic mode ar 10 rad/s and a strain of 1%.
 235000 - 345000 cP
@Temperature 25.0 °C
235000 - 345000 cP
@Temperature 77.0 °F
Measured with parallel plate in dynamic mode ar 10 rads/s and a strain of 1%.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 900 ohm-cm900 ohm-cm70 parts per 100 of NC E1MY-02 in the final compound
 8000 ohm-cm8000 ohm-cm35 parts per 100 of NC E1MY-02 in the final compound
 10000 ohm-cm10000 ohm-cm12 parts per 100 of NC E1MY-02 in the final compound
 40000 ohm-cm40000 ohm-cm12 parts per 100 of NC E1MY-02 in the final compound
 
Descriptive Properties
AspectPaste, black (Master Batch)
Epoxy Equivalent112.2 - 119.5 g/eq
Epoxy Value8.36 - 8.91 eq/kg
Storage Temperature5°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Diamond, Natural
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
Overview of materials for Epoxy/Carbon Fiber Composite
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6
Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes

PNANOCY992 / 108948

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.