MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: High temperature protective coating for graphite.

PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite from very corrosive atmospheres including most molten metals, all acids, and hot ammonia. PBN is an electrical insulator which exhibits a high degree of anisotropy, e.g. good thermal conductor parallel ("ab") to substrate and thermal insulator through thickness ("c").

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 - 2.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 22.0 GPaYoung's modulus
Compressive Strength 220 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+9 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.00 µm/m-°C
@Temperature 20.0 °C
ab direction
Thermal Conductivity 1.50 - 3.00 W/m-Kin "c" direction
 20.0 - 120 W/m-Kin "ab" direction
Maximum Service Temperature, Air 800 °Coxidation limit
Decomposition Temperature 2500 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.50normal spectrum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Microplasmic Anodizing [Ceramic Coating] for Aluminum, Magnesium, Titanium, Zirconium & Composites
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
3M Techical Ceramics MYCROSINT® CD Boron Nitride
Boron Nitride, Cubic BN, (Borazone)
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride

CADV32 / 424

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.