PVC Copolymer Suspension Resin F-186 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-186 has also found success in applications where clarity and increased toughness is required such as solution coatings on various substrates. Information provided by Formosa Plastics Corporation, USA |