MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pressure Seal 14601 Chlorosulfonated Polyethylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 14601 is a 60 durometer black colored general purpose Hypalon elastomer. It exhibits good resistance to petroleum based oil sat elevated temperatures.

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6161
 61
@Treatment Temp. 100 °C,
Time 252000 sec
61
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 63
@Treatment Temp. 150 °C,
Time 252000 sec
63
@Treatment Temp. 302 °F,
Time 70.0 hour
Service Fluid 100
 66
@Treatment Temp. 125 °C,
Time 252000 sec
66
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM OIL #3
Tensile Strength 20.78 MPa3014 psi
 17.934 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
2601.1 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
Service Fluid 100
Elongation, Ultimate 400 %400 %
 270 %
@Treatment Temp. 150 °C,
Time 252000 sec
270 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Service Fluid 100
100% Modulus 1.85 MPa269 psi
Tear Strength 24.9 kN/m142 pliDie B
Compression Set  18.7 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
18.7 %
@Treatment Temp. 158 °F,
Time 22.0 hour
Solid
 69.7 %
@Treatment Temp. 125 °C,
Time 79200 sec
69.7 %
@Treatment Temp. 257 °F,
Time 22.0 hour
Solid
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -49.4 °C-57.0 °F
Shrinkage  -4.30 %
@Treatment Temp. 125 °C,
Time 252000 sec
-4.30 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Volume, ASTM OIL #3
 2.6 %
@Treatment Temp. 150 °C,
Time 252000 sec
2.6 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, Service Fluid 100
 4.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
4.2 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL251 / 318461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.