MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 74G33J NC010 PA66+PA6-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: 33% Glass Reinforced Polyamide 66 + Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 185 MPa26800 psiDAM; ISO 527-1/-2
Elongation at Break 3.5 %3.5 %DAM; ISO 527-1/-2
Tensile Modulus 10.0 GPa1450 ksiDAM; ISO 527-1/-2
Flexural Modulus 5.00 GPa725 ksi50% RH; ISO 178
Poissons Ratio 0.340.34DAM
Charpy Impact Unnotched 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 250 °C482 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FDAM; ISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-(PA66+PA6),GF33,M1GN,S14-100
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66+PA6-GF33<ISO 11469
Polymer(PA66+PA6)-GF33
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
Resin IdentificationPA66+PA6-GF33ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 74G33W BK196 PA66+PA6-GF33
Celanese Zytel® 101 NC010 PA66
Envalior Akulon® Diablo HT-HG6 (K-X07031) PA66+PA6-GF30, Dry, 30% Glass Filled, Heat Stabilized
Akro-Plastic Akromid® C3 GF 30 5 XTC (4499) PA66/6 Dry, 30% Glass Filled
BASF Nypel® RC6024 BK 30% Mineral/Glass Filled PA6 (Dry)

PDSX5364 / 198004

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.