MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Super Asia Polyblend T40C TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: A? FDA?RoHS?REACH?PAHs approval.
B? Medical grade.
C? Low specific gravity.
D? Extra soft, non-sticky and great hand feel.
E? Odorless and non- toxic.

Material Appearance:
Form: Granules
Color: Transparent/ Customized.

Applications: Medical Supplies, Rehabilitation grip ball, Sex toy… etc.

Processing Method: Injection

Information provided by Super Asia Polyblend Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 - 0.930 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37 - 43ASTM D2240
Tensile Strength 6.50 kg(f)/cm²ASTM D412
 4.94 kg(f)/cm²
@Temperature 63.0 °C,
Time 1.80e+6 sec
Heat Resistance; W-O-M
 5.525 kg(f)/cm²
@Temperature 136 °C,
Time 605000 sec
High Temperature Aging; ASTM D573
Elongation at Break 950 %ASTM D412
 722 %
@Temperature 63.0 °C,
Time 1.80e+6 sec
Heat Resistance; W-O-M
 807.5 %
@Temperature 136 °C,
Time 605000 sec
High Temperature Aging; ASTM D573
Rebound 60 %Elasticity; CNS K1392
Tear Strength Test 1.2[kg/cm2], ASTM D624 Die C
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -60.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUPER035 / 305700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.