MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Semi-Red Brass (Valve Metal), UNS C84400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass; Copper Casting Alloy

Material Notes: Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: General hardware, ornamental castings. plumbing supplies and fixtures, low-pressure valves and fittings.

Classified under: Semi-red brasses and leaded semi-red brasses. ASTM B584; formerly ASTM B145-5A

As cast values below are for sand casting. Alloy does not respond to heat treating. Casting shrinkage allowance is 2%

Key Words: 81-3-7-9, CDA 844, ASTM B30 (CA844), ASTM B271, ASTM B505, ASTM B584; ASTM B145-5A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 55
Tensile Strength, Ultimate 235 MPa
Tensile Strength, Yield 105 MPa
@Strain 0.5 %
Elongation at Break 26 %In 50 mm
Modulus of Elasticity 90.0 GPa
Machinability 90 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 11.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000010513 ohm-cm
@Temperature 20.0 °C
16.4% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 260 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 72.5 W/m-K
@Temperature 20.0 °C
Melting Point 840 - 1005 °C
Solidus 840 °C
Liquidus 1005 °C
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.25 %
Copper, Cu 78 - 82 %
Iron, Fe <= 0.40 %
Lead, Pb 6.0 - 8.0 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.020 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.080 %
Tin, Sn 2.3 - 3.5 %
Zinc, Zn 7.0 - 10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
Hydraulic Bronze, UNS C83800, Copper Casting Alloy
Contact Metal, UNS C83300, Copper Casting Alloy
MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze

MC84400b1 / 11904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.