MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Ovation Polymers Nemcon™ H PO DP 117/X2 Polyolefin, Thermally conductive
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Available as an injection moldable grade to replace metals in enclosures and medical device parts. It should be used in applications where thermal management must be accomplished.

All properties after 48hrs conditioning at 23°C/50% RH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12.0 MPa50 mm/min; ASTM D638
Elongation at Break 5.2 %50 mm/min; ASTM D638
Tensile Modulus 450 MPa50 mm/min; ASTM D638
Flexural Strength 20.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.370 GPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.400 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 5.00e+12 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.30 W/m-KASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
@Thickness 3.20 mm
Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers Nemcon™ H PA DP117/X3 Polyphthalamide, Thermally Conductive
Ovation Polymers Nemcon™ H PC DP120/X2 Polycarbonate, Thermally Conductive
Ovation Polymers Nemcon™ H PC DP120/X3 BK Polycarbonate, Thermally Conductive, Black
Ovation Polymers Nima™ NH PC143P Polycarbonate
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound

POVAT138 / 79117

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.