MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 1783 Modified Polyphenylene Oxide (PPO); Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D 792
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.0010 cm/cm
@Thickness 3.20 mm
0.0010 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 84.1 MPa12200 psiASTM D 638
Elongation at Break 1.0 %1.0 %ASTM D 638
Tensile Modulus 13.1 GPa1900 ksiASTM D 638
Flexural Strength 107 MPa15500 psiASTM D 790
Flexural Modulus 11.7 GPa1700 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 1.87 J/cm
@Thickness 3.20 mm
3.50 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10 ohm-cm<= 10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  25 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
25 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 26 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
26 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 26 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
26 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 28 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
28 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 30 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
30 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 31 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
31 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 288 °C480 - 550 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 93.3 °C
@Time 7200 sec
200 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1701 MG 20  Modified Polyphenylene Oxide (PPO) Glass Fiber 10% - Milled Glass 20%
RTP Company RTP 1701 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free
RTP Company RTP 1700 TFE 15 Modified Polyphenylene Oxide (PPO), PTFE Lubricated
RTP Company RTP 1700 TFE 13 SI 2 Modified Polyphenylene Oxide (PPO), PTFE Lubricated - Silicone Lubricated
RTP Company RTP 1700 TFE 10 FR Modified Polyphenylene Oxide (PPO), PTFE Lubricated - Flame Retardant

PQZRA37009 / 205907

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.