MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt POLYCOR® 23 X Series Gel Coat
Categories: Polymer; Thermoset

Material Notes: 23X series of gelcoats are formulated specifically for composite mold making. It is formulated with a special base resin that permits an excellent resistance to heat distortion even after repeated use. They provide a high gloss and hard durable surface. These tooling gel coats are formulated ready-to-spray after the addition of the proper amount of appropriate methyl ethyl ketone peroxide or cumene hydro peroxide catalyst. The « low opacity» formulation help to detect default during spraying process. See section: «application» in PB-5 (Polyester tooling) because even though manufacturing precautions are used to make tooling gelcoat, a misapplication of these products can produce unacceptable results.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 - 1.13 g/cc
Brookfield Viscosity 4500 - 5500 cPRVF #4 Spindle @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 40 - 55tested with 40 grams mass @ 25°C catalyzed at 1,8%
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 144 °Cbefore post cure; Catalyzed with 1,8% NOROX CHM50; residual heat: 48 J/g
 151 °Cafter a post cure 4 hours @ (65°C); Catalyzed with 1,8% NOROX CHM50; residual heat: 23 J/g
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 50.0 minLay-up Time
Gel Time 14.0 - 20.0 min
@Temperature 25.0 °C
tested with 100 grams mass @ 25°C catalyzed at 1,8% NOROX CHM50
 
Descriptive Properties
Thixotropic Index5-72/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9261 / 231856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.