MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 980 Fluorosilicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Superior chemical resistance
  • Excellent physical strength
  • Addition cured type system
  • Highly flexible & temperature resistant
Product Description: Master Bond MasterSil 980 is a two component fluorosilicone for bonding, sealing, coating and encapsulating. Its most outstanding attribute is enhanced chemical resistance particularly to fuels, oils and solvents when compared to conventional silicones. Noteworthy in this regard, is its ability to withstand gasoline, diesel fuel, motor oil, ethanol and many other alcohols, among others. (A more detailed description is presented in the chart below.) MasterSil 980 is an addition cured system that does not require air or humidity for curing. The mix ratio is 100 to 10 by weight and after mixing it is a moderate viscosity liquid with good flow. Its open time is certainly user friendly; 6-9 hours at room temperature for a 50 gram mass. The cure schedule is 30-60 minutes at 260-300°F or 75-90 minutes at 200-250°F. MasterSil 980 is a superior bonding agent and it adheres well to many substrates including metals, composites, ceramics, glass as well as many rubbers and plastics. MasterSil 980 can withstand the most aggressive types of thermal cycling as well as mechanical and thermal shock. After curing, MasterSil 980 is a good electrical insulator and can be used for potting and encapsulation. It can be used as a formed-in-place gasketing material. Also, this product bonds well to other silicone substrates. The system is 100% solids and contains no solvents or diluents. The color of Part A is red and Part B is white. The service temperature range is -85°F to +465°F. In summary, MasterSil 980 retains silicone type flexibility and temperature resistance; along with significantly raising the level of chemical resistance. MasterSil 980 is a good candidate for applications in the aerospace, electronic, specialty OEM and chemical processing industries, among others, where the silicone product property profile along with enhanced chemical resistance is desirable.

Product Advantages:

  • Convenient working life after mixing
  • Good flow properties
  • Excellent adhesive
  • Cures well in deep and wide sections
  • Best chemical resistance for a silicone based system

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccmixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 30
Tensile Strength 150 - 350 psi
Elongation at Break 100 - 200 %
Adhesive Bond Strength 100 - 300 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 6.4
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 465 °F
Minimum Service Temperature, Air -85.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 60.0 min
@Temperature 127 - 149 °C
 75.0 - 90.0 min
@Temperature 93.3 - 121 °C
Working Life 360 - 540 minAfter mixing, 50 gram batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Chemical ResistanceAcetoneFair
 Brake fluidExcellent
 Crude oilGood
 Diesel fuelFair
 EthanolFair to good
 Ethylene glycolGood
 GasoholFair
 GasolineGood
 Isopropyl alcoholGood
 JP4 jet fuelGood to excellent
 Mineral oilExcellent
 Potassium hydroxide 25%Excellent
 SAE no. 20 oilGood
 Skydrol 500BExcellent
 Sodium hydroxide 25%Good
 SteamNot recommended
 Sulfuric acid 30%Good
 TolueneNot recommended
 WaterExcellent
 XyleneNot recommended
Mixing Ratio100:10 by weightPart A to B
Viscositymoderate flowmixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering N55E Nitrile Rubber
Precision Polymer Engineering N60C Nitrile Rubber
Precision Polymer Engineering N60K Nitrile Rubber
Dow 5-8601 FLUOROSILICONE LSR, KIT
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER

PMASTM948 / 185541

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.