MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QM 2223 23 Shore A, Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 2223 is a two-component, room temperature, condensation cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where high durometer, dimensional stability and extremely tough rubber are required. A variety of catalysts are offered with this material.

Key Features:

  • Low specific gravity
  • Low viscosity
  • Long work-life
  • Fast demold time
  • Excellent flowability
Main Applications:
  • Molds for large and small statues
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication
  • Molds for GFRC pre-cast

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccUncatalyzed MM Purple
 1.00 g/ccUncatalyzed MM Green
 1.00 g/ccUncatalyzed MM Blue
 1.00 g/ccUncatalyzed MM Red
 1.02 g/ccCatalyzed MM Blue
 1.05 g/ccCatalyzed MM Purple
 1.05 g/ccCatalyzed MM Green
 1.09 g/ccCatalyzed MM Red
 1.16 g/ccUncatalyzed QM 2223
Viscosity 150 cPUncatalyzed MM Purple
 150 cPUncatalyzed MM Green
 150 cPUncatalyzed MM Blue
 150 cPUncatalyzed MM Red
 32000 cPCatalyzed MM Purple
 32000 cPCatalyzed MM Green
 32000 cPCatalyzed MM Blue
 32000 cPCatalyzed MM Red
 50000 cPUncatalyzed QM 2223
Linear Mold Shrinkage <= 0.0025 cm/cmCured 3 days RT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 23Cured 3 days RT
Tensile Strength 400 psiCured 3 days RT
Elongation at Break 350 %Cured 3 days RT
Tear Strength 30.0 pliCured 3 days RT
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 8.00 hourDemold time, Catalyzed MM Blue
 6.00 - 8.00 hourDemold time, Catalyzed MM Red
 8.00 - 10.0 hourDemold time, Catalyzed MM Purple
 8.00 - 10.0 hourDemold time, Catalyzed MM Green
 72.0 hour
@Temperature 25.0 °C
Tack-Free Time 3.00 - 5.00 hourCatalyzed MM Blue
 4.00 - 6.00 hourCatalyzed MM Red
 4.00 - 6.00 hourCatalyzed MM Purple
 4.00 - 6.00 hourCatalyzed MM Green
Pot Life 30.0 minCatalyzed MM Blue
 30.0 minCatalyzed MM Red
 60.0 minCatalyzed MM Purple
 60.0 minCatalyzed MM Green
 
Descriptive Properties
ColorBlueUncatalyzed MM Blue
 GreenUncatalyzed MM Green
 Light BlueCatalyzed MM Blue
 Light GreenCatalyzed MM Green
 Light PurpleCatalyzed MM Purple
 Light RedCatalyzed MM Red
 PurpleUncatalyzed MM Purple
 RedUncatalyzed MM Red
 WhiteUncatalyzed QM 2223

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems QuickPlastic Cast Urethane Material Elastomer 25 A
CHT Group MM925 Condensation Cure 2-Part Molding Rubber
CHT Group QM 2225 25 Shore A, Condensation Cure Moldmaking Material
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Overview of materials for Silicone Rubber

PACC2044 / 199432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.