Data provided by the manufacturer, Exxon Chemical. A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in bag making equipment. Film made from LD-113 generally can be drawn down to 0.75 mils. Applications: Refuse and trash bags; Drum and box liners; Rack and counter bags; Light duty produce bags; Other general purpose packaging and non-packaging applications. Data for film properties below based on 1.25 mil film. |
Low Density Polyethylene; Exxon Chemical Company |