Application: Crosslinking agent for free radical polymerization. Adhesion promoter and hardener for PVC plastisols. Coagent for peroxide crosslinking of elastomers. Appearance: Clear to slight turbid, yellowish liquid Odor: Faintly ester-like CAS: 3290-92-4 Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |