MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Varcum 29358 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29358 is used in the manufacturing of grinding wheels.

DESCRIPTION: Varcum 29358 is a one-step liquid phenolic resin.

FEATURES:

  • An excellent wetting agent for the production of abrasive mixes for grinding wheel manufacture.
  • A higher viscosity version of our standard, general purpose liquid resin wetting agent Varcum 29353.
  • Provides optimum and uniform wetting of the abrasive grain and powdered resin components.
  • The higher non-volatile content of this resin reduces the problems of wheel distortion due to the evolution of volatiles during the baking cycle.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 8.35DCT 4064A
Viscosity 1400 cP
@Temperature 25.0 °C
DCT 4003F
 
Descriptive Properties
Non Volatile (%)77DCT 4005A
Water Tolerance (%)175DCT 4012A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Phenolic; Unreinforced; Molded
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Overview of materials for Phenolic, Carbon Fiber Composite

PSUMIT710 / 194515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.