MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchkote™ 152LV Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Coating 152LV has been specifically developed as a surface tolerant anti corrosive coating for steel structures.

Product Features:

  • Combines good application characteristics with excellent corrosion protection and chemical resistance.
  • Is designed for application by brush at thicknesses of up to 1mm in a single application.
  • Is suitable for use on grit blasted steel, mechanically prepared steelwork or high pressure water cleaned steel.
  • Adhesion: Excellent to both blast cleaned and mechanically prepared surfaces.
  • Corrosion: Resistance Excellent even under immersion conditions.
  • Chemical Resistance: Unaffected by short term contact with most industrial chemicals.
  • Temperature Resistance: Suitable for use up to 100°C dry heat

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
Solids Content 99.2 %99.2 %
Volatile Organic Compounds (VOC) Content 14 g/l14 g/lmixed
Thickness 254 - 1020 microns10.0 - 40.0 mil
 
Processing PropertiesMetricEnglishComments
Cure Time 720 min12.0 hourTouch Dry
 960 min16.0 hourHard Dry
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceBeige, gray or black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35289 / 170036

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.