MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Morgan Advanced Ceramics High Strength Ceramic Fibre Boards HS-45 Ceramic Fibre Boards
Categories: Ceramic; Oxide

Material Notes: High strength ceramic fibre Boards are having high compressive and flexural strength and good resistance to erosion from gas flow than normal Ceramic fiber boards. High strength Boards are designed to meet the toughest knocks and pressure maintaining its strength over a long productive life. It has low shrinkage compared to other fibre products.

Applications:

  • Backup insulation in steel ladles Like Tundish & Torpedo ladles.
  • Rotary Kiln back up of calcining and dolomite Kiln.
  • Used as back up to feeder channels of glass tanks.
  • Excellent Non – wettability to molten Aluminum and ideally suited for various molten metal contact applications such as Launders, Header Box, Troughs and Hot top Moulds etc

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.720 g/cc0.0260 lb/in³
Loss On Ignition >= 10 %>= 10 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00200 GPa0.290 ksi> 25mm thick
 0.00300 GPa0.435 ksi< 25mm thick
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.160 W/m-K
@Temperature 600 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C201
Shrinkage 1.0 %1.0 %ENV 1094-7
 
Component Elements PropertiesMetricEnglishComments
Al2O3 49 - 53 %49 - 53 %IS: 12107/XRF
CaO 9.0 - 12 %9.0 - 12 %IS: 12107/XRF
SiO2 33 - 37 %33 - 37 %IS: 12107/XRF
 
Descriptive Properties
Classification Temperature (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 510°C (950°F) for 3 hours, 3.18 mm sheet

CMORF6491 / 203275

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.