MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Impact modified, UV stabilized

The exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low weight is desired. Hybrid Plastics offers POSS-modified COC plastics that are tough, weather resistant and easily processed. These materials do not use fillers. They exhibit some of the highest heat distortion temperatures at the lowest densities available on the market. Other modifications are available.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 13 %13 %
Flexural Modulus  1.70 GPa
@Temperature 130 °C
247 ksi
@Temperature 266 °F
 2.40 GPa
@Temperature 40.0 °C
348 ksi
@Temperature 104 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 155 °C311 °F
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 270 °C464 - 518 °F
Middle Barrel Temperature 250 - 300 °C482 - 572 °F
Front Barrel Temperature 260 - 310 °C500 - 590 °F
Nozzle Temperature 250 - 310 °C482 - 590 °F
Mold Temperature 90.0 - 115 °C194 - 239 °F
 
Descriptive Properties
ColorDark Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® COC BLEND-15GF Natural Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer
Polyplastics TOPAS® Elastomer E-140 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)

PHYBR034 / 88742

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.