MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Novec™ 2702 Electronic Grade Coating
Categories: Polymer

Material Notes: 3M™ Novec™ 2702 Electronic Grade Coating is designed for protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical polymer coating carried in a hydrofluoroether solvent. The coating is easy to apply and should be heat cured.

Features and Benefits:

  • Low surface tension of the coating solution provides increased surface wetting, especially under low profile components
  • Cross-links with a thermal cure for durable protection
  • Contains no volatile organic compounds (VOCs) and has low global warming potential
  • Can be applied to metals, glass or epoxy laminates
  • Provides excellent repellency, anti-wetting and anti-sticking properties against liquids ie: water, hydrocarbons, silicones, and photoresists

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³
Solids Content 2.0 %2.0 %fluoropolymer
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.61
@Frequency 1e+6 Hz
2.61
@Frequency 1e+6 Hz
 3.04
@Frequency 1000 Hz
3.04
@Frequency 1000 Hz
 3.45
@Frequency 10 Hz
3.45
@Frequency 10 Hz
Dielectric Strength 59.1 kV/mm1500 kV/in30% RH
Dissipation Factor  0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
 0.040
@Frequency 1000 Hz
0.040
@Frequency 1000 Hz
 0.050
@Frequency 10 Hz
0.050
@Frequency 10 Hz
 
Thermal PropertiesMetricEnglishComments
Boiling Point 76.0 °C169 °Fof Solvent
Glass Transition Temp, Tg -63.0 °C-81.4 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.411.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 71DA Engineered Fluid
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid

PMM33102 / 167849

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.