MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Overview of materials for Refractory Metal
Categories: Metal; Nonferrous Metal; Refractory Metal

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Refractory Metal". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 - 21.0 g/ccAverage value: 14.5 g/cc Grade Count:384
Particle Size 1.10 - 40.0 µmAverage value: 12.7 µm Grade Count:11
 
Chemical PropertiesOriginal ValueComments
Thermal Neutron Cross Section 1.10 - 86.0 barns/atomAverage value: 23.8 barns/atom Grade Count:18
Electrode Potential -1.10 - 4.50 VAverage value: 2.46 V Grade Count:9
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 95.0 - 2550Average value: 471 Grade Count:29
Hardness, Knoop 175 - 505Average value: 268 Grade Count:8
Hardness, Rockwell A 35.0 - 76.0Average value: 60.6 Grade Count:14
Hardness, Rockwell B 25.0 - 110Average value: 81.4 Grade Count:116
Hardness, Rockwell C 12.0 - 50.0Average value: 30.9 Grade Count:83
Hardness, Vickers 50.0 - 550Average value: 246 Grade Count:82
Vickers Microhardness 65.0 - 140Average value: 99.2 Grade Count:3
Tensile Strength, Ultimate 112 - 4900 MPaAverage value: 755 MPa Grade Count:219
Tensile Strength, Yield 72.4 - 1640 MPaAverage value: 565 MPa Grade Count:161
Elongation at Break 0.000 - 70.0 %Average value: 12.3 % Grade Count:170
Reduction of Area 32.0 - 54.0 %Average value: 42.3 % Grade Count:4
Modulus of Elasticity 68.9 - 469 GPaAverage value: 282 GPa Grade Count:144
Compressive Yield Strength 351 - 683 MPaAverage value: 604 MPa Grade Count:9
Poissons Ratio 0.200 - 0.380Average value: 0.306 Grade Count:25
Fatigue Strength 230 - 465 MPaAverage value: 342 MPa Grade Count:11
Machinability 75.0 - 80.0 %Average value: 78.8 % Grade Count:4
Shear Modulus 37.3 - 176 GPaAverage value: 114 GPa Grade Count:25
Shear Strength 250 - 425 MPaAverage value: 331 MPa Grade Count:4
Charpy Impact 4.70 - 160 JAverage value: 56.2 J Grade Count:10
Charpy Impact, Unnotched 12.2 - 210 JAverage value: 120 J Grade Count:10
Charpy Impact, Notched 30.0 - 170 J/cm²Average value: 97.5 J/cm² Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000190 - 0.0000290 ohm-cmAverage value: 0.00000819 ohm-cm Grade Count:216
Magnetic Permeability 1.05Average value: 1.05 Grade Count:24
Magnetic Susceptibility 3.30e-7 - 0.00000228Average value: 0.00000111 Grade Count:9
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.40 - 12.8 µm/m-°CAverage value: 6.49 µm/m-°C Grade Count:146
Specific Heat Capacity 0.132 - 0.340 J/g-°CAverage value: 0.221 J/g-°C Grade Count:63
Thermal Conductivity 0.0581 - 330 W/m-KAverage value: 134 W/m-K Grade Count:201
Melting Point 810 - 3420 °CAverage value: 2500 °C Grade Count:148
Solidus 810 - 1430 °CAverage value: 1080 °C Grade Count:61
Liquidus 851 - 3410 °CAverage value: 3040 °C Grade Count:76
Boiling Point 4610 - 5900 °CAverage value: 5240 °C Grade Count:33
Maximum Service Temperature, Air 500 - 2760 °CAverage value: 1680 °C Grade Count:15
Minimum Service Temperature, Air 0.000 °CAverage value: 0.000 °C Grade Count:5
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.420 - 0.490Average value: 0.455 Grade Count:4
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 1600 - 2050 °CAverage value: 1850 °C Grade Count:3
Recrystallization Temperature 900 - 2600 °CAverage value: 1680 °C Grade Count:14
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.000100 - 0.0100 %Average value: 0.00247 % Grade Count:44
Cadmium, Cd 0.000100 - 0.00150 %Average value: 0.00111 % Grade Count:16
Calcium, Ca 0.000100 - 0.0100 %Average value: 0.00250 % Grade Count:34
Carbon, C 0.00100 - 0.150 %Average value: 0.0147 % Grade Count:86
Chlorine, Cl 0.000100 - 0.000500 %Average value: 0.000200 % Grade Count:4
Chromium, Cr 0.000100 - 10.0 %Average value: 0.171 % Grade Count:58
Cobalt, Co 0.000100 - 35.0 %Average value: 4.38 % Grade Count:8
Copper, Cu 0.000100 - 69.0 %Average value: 16.7 % Grade Count:158
Fe + Ni 1.50 - 10.0 %Average value: 5.30 % Grade Count:5
Hafnium, Hf 0.000100 - 30.0 %Average value: 5.17 % Grade Count:17
Hydrogen, H 0.000500 - 0.0100 %Average value: 0.00150 % Grade Count:27
Iron, Fe 0.000100 - 13.5 %Average value: 0.758 % Grade Count:123
Lanthanum, La 0.150 - 1.20 %Average value: 0.758 % Grade Count:7
Lead, Pb 0.000100 - 0.00200 %Average value: 0.00128 % Grade Count:30
Lithium, Li 0.000100 %Average value: 0.000100 % Grade Count:4
Magnesium, Mg 0.000100 - 0.0100 %Average value: 0.00131 % Grade Count:35
Manganese, Mn 0.000100 - 0.00500 %Average value: 0.00115 % Grade Count:21
Molybdenum, Mo 0.000500 - 100 %Average value: 67.3 % Grade Count:132
Ni, Fe, Mo 7.00 - 10.0 %Average value: 7.60 % Grade Count:5
Nickel, Ni 0.000100 - 47.2 %Average value: 2.68 % Grade Count:143
Niobium, Nb (Columbium, Cb) 0.00100 - 100 %Average value: 57.8 % Grade Count:41
Nitrogen, N 0.00100 - 0.0300 %Average value: 0.00633 % Grade Count:58
Oxygen, O 0.00150 - 0.500 %Average value: 0.0533 % Grade Count:79
Palladium, Pd 34.0 - 65.0 %Average value: 51.4 % Grade Count:4
Phosphorus, P 0.000900 - 0.00200 %Average value: 0.00163 % Grade Count:3
Potassium, K 0.000100 - 0.0150 %Average value: 0.00506 % Grade Count:47
Rhenium, Re 1.50 - 100 %Average value: 29.5 % Grade Count:20
Silicon, Si 0.000100 - 6.10 %Average value: 0.0821 % Grade Count:87
Silver, Ag 0.000500 - 90.0 %Average value: 37.2 % Grade Count:49
Sodium, Na 0.000100 - 0.0100 %Average value: 0.00193 % Grade Count:32
Sulfur, S 0.000100 - 0.150 %Average value: 0.0194 % Grade Count:8
Tantalum, Ta 0.00200 - 100 %Average value: 69.3 % Grade Count:53
Thorium, Th 5.00e-7 - 4.00 %Average value: 1.38 % Grade Count:12
Tin, Sn 0.000100 - 0.00800 %Average value: 0.00232 % Grade Count:34
Titanium, Ti 0.000100 - 44.0 %Average value: 1.37 % Grade Count:43
Tungsten, W 0.00100 - 100 %Average value: 68.7 % Grade Count:324
Uranium, U 5.00e-7 %Average value: 5.00e-7 % Grade Count:4
Vanadium, V 0.000100 - 25.0 %Average value: 4.17 % Grade Count:6
WC 50.0 - 70.0 %Average value: 56.5 % Grade Count:4
Yttrium, Y 0.000100 - 0.300 %Average value: 0.0352 % Grade Count:5
Zinc, Zn 0.000100 - 0.00100 %Average value: 0.000533 % Grade Count:9
Zirconium, Zr 0.000100 - 3.00 %Average value: 0.386 % Grade Count:31
ZrO2 0.0700 - 1.70 %Average value: 0.690 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Overview of materials for Cobalt Alloy
Overview of materials for Molybdenum Alloy
Overview of materials for Tungsten Alloy
Overview of materials for Stainless Steel

M01067 / 81676

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.