MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 2315A Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Impact Copolymer with Nucleating, Antistat Additives

Applications: Injection Molded Caps and Closure Applications

Formolene 2315A is a copolymer of polypropylene designed and formulated for injection molded caps and closure applications. It contains a unique combination of stabilizers, nucleators and antistats that give it an excellent balance of stiffness and impact strength. Formolene 2315A offers advantages in both processing and physical properties over current polypropylenes used for injection molded caps and closures.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Specimens were injection molded according to the conditions specified in ASTM D4101.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D1505
Melt Flow 15 g/10 min
@Temperature 230 °C
I2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength, Yield 4400 psi2" (50mm) per min.; ASTM D638
Elongation at Yield 4.5 %2" (50mm) per min.; ASTM D638
Flexural Modulus, 1% Secant 240000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 1.70 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 2325N Injection Applications Polypropylene
Formosa Plastics Formolene® 2510A Injection Applications Polypropylene
Formosa Plastics Formolene® 2520A Injection Molding Polypropylene
Braskem H 201 Injection Molding Polypropylene
Formosa Plastics Formolene® 2515N Injection Molding Polypropylene

PFPCPP33 / 38889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.