MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PVDF-ELS Polyvinylidene Fluoride, Electrically Conductive
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechanical strength and toughness at lower temperature and it's self-extinguishing. The temperature ranges from -30°C to 150°C.

Properties

  • high tensile strength
  • high mechanical strength
  • high rigidity
  • high chemical resistance
  • very low water absorption
  • good friction and wear and tear values
  • self-extinguishing
  • high UV-resistance
  • toxic fumes when burned
  • can not be solvent cemented
  • relatively high coefficient of thermal expansion
Applications include gaskets, pumps, rotation disks, valves, flap traps, centrifugals of extraction, fittings, glide tracks, and cogwheels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/ccISO 1183
Moisture Absorption at Equilibrium 0.040 %ISO 62
Water Absorption at Saturation 0.10 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76ISO 868
Tensile Strength, Yield 40.0 MPaISO 527
Elongation at Break >= 20 %ISO 527
Elongation at Yield 9.0 %ISO 527
Modulus of Elasticity 1.60 GPaISO 527
Charpy Impact, Notched 8.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10000 ohm-cmIEC 60093
Surface Resistance <= 10000 ohm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°CISO 11359
Maximum Service Temperature, Air 150 °CUL 746B
Minimum Service Temperature, Air -30.0 °CUL 746B
 
Compliance PropertiesOriginal ValueComments
FDA NoPhysiological indifference
 
Descriptive Properties
Acid Resistancelimited
Bondabilitylimited
Colorblack
Physiological indifferenceno, EEC
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-202 Conductive Polyimide
Arkema Pebax® 5533 SN 70 BLACK Polyether Block Amide (PEBA) (Dry)
CENTROPLAST CENTROFLON Polyvinylidene fluoride
EMS-Grivory Grilamid® L 20 EC PA12-CD25
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled

PGEHR030 / 79867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.