MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear ATF Type F Automatic Transmission Fluid is a high-static-friction fluid developed for Ford automatic transmissions manufactured during the 1960s and 1970s. (Newer Ford transmissions require MERCON® automatic transmission fluid.) The special frictional qualities of ATF Type F ensure proper shifting in Ford transmissions that require an ESW-M2C33-F fluid. It is also recommended for power steering systems in a wide variety of Ford vehicles. Hydroclear ATF Type F resists foaming to protect against rust, corrosion, wear and deposits. Its low viscosity suits it not only for Ford power-steering units, but also as a hydrostatic drive fluid for most farm tractors and combines. It is dyed red for easy identification.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.7 °
Viscosity Measurement 180Viscosity Index
Saybolt Viscosity at 100°F 200 SUS
Saybolt Viscosity at 210°F 54 SUS
Kinematic Viscosity at 40°C (104°F) 43 cSt
Kinematic Viscosity at 100°C (212°F) 7.6 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -43.0 °F
Flash Point 365 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
ChevronTexaco Type F Automatic Transmission Fluid
ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid
ChevronTexaco MERCON® V Automatic Transmission Fluid
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid

WCON027 / 75064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.