MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mar-Bal AltraSet MB4000 Thermoset Polyester - Superior Tracking Resistance Grade
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: MB4000 is the best high track resistant material in the AltraSet product line. It is a flame retardant polyester molding compound with moderate strength, excellent electrical properties and exceptional arc and track resistance. Used where higher track resistance is critical – such as porcelain replacement in insulators or other electrical applications.

Key features include Incline Plane Tracking of over 1,500 minutes and rated UL 94 5VA @1.65mm. UL file number E80533

Information provided by Mar-Bal, Inc.

Vendors: Mar-Bal is the leading integrated compounder and molder of BMC Thermoset composite products and value added finishing services. Call 440-543-7526 or visit Mar-Bal.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.70 - 1.90 g/cc0.0614 - 0.0686 lb/in³ASTM D792
Water Absorption 0.12 %0.12 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.030 cm/cm0.0050 - 0.030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 41 - 4741 - 47ASTM D2583
Tensile Strength 62.1 - 68.9 MPa9000 - 10000 psiASTM D638
Flexural Strength 114 - 124 MPa16500 - 18000 psiASTM D790
Flexural Modulus 11.7 - 13.1 GPa1700 - 1900 ksiASTM D790
Compressive Strength 145 - 165 MPa21000 - 24000 psiASTM D695
Izod Impact, Notched 5.07 - 5.61 J/cm9.50 - 10.5 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 13.8 kV/mm>= 350 kV/inASTM D149
Arc Resistance >= 185 sec>= 185 secASTM D495
Track Resistance >= 90000 sec>= 90000 secInclined-Plane Tracking; ASTM D2303-85
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
UL RTI, Electrical 130 °C266 °FUL746B
UL RTI, Mechanical with Impact 130 °C266 °FUL746B
UL RTI, Mechanical without Impact 130 °C266 °FUL746B
Flammability, UL94 5VA
@Thickness 1.65 mm
5VA
@Thickness 0.0650 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound

PMARB860 / 233843

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.