Kraton MD1537 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is manufactured in North America and has the following characteristics: Kraton MD1537 H is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens. Development product. Kraton MD1537 HU - supplied as a powder. Information provided by Kraton Corporation. |