MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound 5C003 Polyvinylidene Fluoride (PVDF)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: LNP THERMOCOMP 5C003 compound is based on Polyvinylidene Fluoride (PVDF) resin containing 15% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³ISO 1183
 1.769 g/cc0.06391 lb/in³ASTM D792
Moisture Absorption 0.0300 %0.0300 %23°C/50% RH/24 hrs; ASTM D570
 0.0400 %0.0400 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/in24hrs; ISO 294
 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.013 cm/cm0.010 - 0.013 in/in24hrs; ASTM D955
 0.0116 cm/cm0.0116 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 67.0 MPa9720 psiISO 527
 78.0 MPa11300 psiASTM D638
Elongation at Break 0.60 %0.60 %ISO 527
 0.80 %0.80 %ASTM D638
Tensile Modulus 14.27 GPa2070 ksi5 mm/min; ASTM D638
 14.5 GPa2100 ksi1 mm/min; ISO 527
Flexural Strength 127 MPa18400 psiASTM D790
 147 MPa21300 psiISO 178
Flexural Modulus 11.79 GPa1710 ksiASTM D790
 20.92 GPa3034 ksiISO 178
Izod Impact Notched 58.0 J42.8 ft-lbASTM D256
Izod Impact, Unnotched 2.02 J/cm3.78 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 14.0 kJ/m²6.66 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 11.0 J8.11 ft-lbpeak; ASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  31.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 31.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  86.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 86.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 165 °C329 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 165 °C
@Thickness 3.20 mm
329 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 156 °C313 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 159 °C
@Thickness 3.20 mm
318 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 210 - 225 °C410 - 437 °F
Zone 3 225 - 245 °C437 - 473 °F
Melt Temperature 215 - 230 °C419 - 446 °FInjection Molding
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81440 / 289387

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.