System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Wieland 1757 Wilaform Platinum
Categories:
Metal
;
Nonferrous Metal
;
Precious Metal
;
Platinum Alloy
Material Notes:
Platinum alloy without nickel, low-priced for all kinds of decoration production
Applications: chains, laminar decoration, pipes, tubing
Dental
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
21.5
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Vickers
160
HV5; glowed
Thermal Properties
Original Value
Comments
Melting Point
1800
-
1820
°C
Solidus
1800
°C
Liquidus
1820
°C
Processing Properties
Original Value
Comments
Casting Temperature
1950
-
2150
°C
Component Elements Properties
Original Value
Comments
Iridium, Ir
15 %
Platinum, Pt
85 %
Descriptive Properties
Color
platinum-white
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Wieland 1951 Wilaform Platinum
Overview of materials for Platinum Alloy
Johnson Matthey SW 900 Platinum w/ 10% Iridium Jewelry Alloy
Goodfellow Platinum 90/Iridium 10 Alloy
NWIELAN79 / 19881
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.