MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 8777 Sealing Tape
Categories: Polymer; Tape

Material Notes: 3M™ Sealing Tape 8887 is a self-adhered, waterproof membrane designed for sealing on difficult to stick to surfaces. This product has a unique acrylic pressure sensitive adhesive that aggressively sticks and stays stuck both at lower and higher application temperatures. The proprietary backing seals around hand driven nails and staples to prevent moisture intrusion. This backing is tough, resist punctures and tears, yet it is thin and conformable to fit conveniently into corners.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 251 microns9.90 milASTM D3752
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.5478 kN/m3.125 pliAdhesion to Housewrap; ASTM D3330
 0.657 kN/m3.75 pliAdhesion to Polyethylene; ASTM D3330
 0.657 kN/m3.75 pliAdhesion to OSB; ASTM D3330
 0.657 kN/m3.75 pliAdhesion to Anodized Aluminum, after UV Exposure; ASTM D3330
 0.71216 kN/m4.0625 pliAdhesion to Anodized Aluminum, after 7 days in water; ASTM D3330
 0.7669 kN/m4.375 pliAdhesion to Anodized Aluminum, after 7 days at 176°F; ASTM D3330
 0.82172 kN/m4.6875 pliAdhesion to Anodized Aluminum, after Thermal Cycling; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -18.0 °C>= -0.400 °FApplication
 <= 49.0 °C<= 120 °FApplication
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34543 / 169290

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.