MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 40% Glass Filled; Polyphenylene Ether, Heat Resistant

Material Notes: Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame Retardant

Features: • Bromine Free • Chlorine Free • Self Extinguishing
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
Melt Flow 1.0 - 9.0 g/10 min
@Load 11.6 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength at Break 18300 psiASTM D638
Tensile Strength, Yield 18300 psiASTM D638
Elongation at Yield 1.5 %ASTM D638
Flexural Strength 23000 psiASTM D790
Flexural Modulus 1400 ksiASTM D790
Izod Impact, Notched 1.30 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 235 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 250 °FASTM D648
Flammability, UL94 V-1
@Thickness 1.59 mm
 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 580 °F
Middle Barrel Temperature 520 - 590 °F
Front Barrel Temperature 540 - 600 °F
Melt Temperature 560 - 600 °F
Mold Temperature 170 - 220 °F
Drying Temperature 220 - 230 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00150 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade
MTM Plastics Dipolen® S Recycled PP + PE Blend
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy

PPOLYQ239 / 160763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.