Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat Stabilized Appearance: Black Processing Method: Injection Molding Information provided by TP Composites, Inc. |