MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAPEAK XW3720 (FE210103) PEEK, 20% PTFE Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, PTFE-Filled

Material Notes: PEEK tribologically modified with 20 % PTFE

Properties: dimensionally stable, good gliding properties, good aging behavior, good fire behavior, High strength, High wear resistance, Very high continuous used temperature, semi-crystalline

Typical areas of application: Fasteners, Housing, Sliding elements, Piston, Rotors, Bobbin, Plug, Valves, Gears

Industries: Automotive, Electrical and electronics industry, Household appliances, Aviation Industry, Mechanical Engineering, Medical Technology

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183-1
Water Absorption 0.300 %0.300 %ISO 62
Linear Mold Shrinkage, Flow 0.0120 cm/cm0.0120 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0170 cm/cm0.0170 in/inISO 294-4
Melt Flow 8.00 g/10 min
@Load 5.00 kg,
Temperature 380 °C
8.00 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 81.081.0DIN ISO 7619-1
Tensile Strength, Yield 75.0 MPa10900 psiISO 527-1
Elongation at Break 25.0 %25.0 %ISO 527-1
Elongation at Yield 6.50 %6.50 %ISO 527-1
Modulus of Elasticity 3.00 GPa435 ksiISO 527-1
Compressive Strength 105 MPa15200 psiISO 604
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmContact; IEC 60093
Dielectric Strength 21.0 kV/mm533 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FISO 11357-1/-3
Glass Transition Temp, Tg 143 °C289 °FDIN EN ISO 11357-1
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FInjection
Melt Temperature 365 - 400 °C689 - 752 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 150 - 160 °C302 - 320 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO685 / 326759

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.