MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Vac-Pak® E4760 Release Film
Categories: Polymer; Film

Material Notes: Description: Release film. Ideally suited to aerospace applications.

Features & Benefits:

  • Clear or blue tinted modified polymer release film providing excellent release capabilities from epoxy, phenolic, polyester and other resin system without contamination
  • Specifically developed for use in mild contours and flat panel applications
  • With 300% and 204°C (400°F) capabilities, this is an economical alternative
  • Available perforated or non-perforated

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 38.0 microns
 51.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4400 psi
Elongation at Break 300 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
 
Descriptive Properties
ColorClear and blue
Yield46.6 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay A2000 Release Film
Kolon CY412 Silicone Release Film
Solvay E2760 Release Film
Solvay Vac-Pak® E7760W Release Film
Solvay Vac-Pak® E3760 PVF Release Film

PCYTED278 / 180580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.