MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eneos RB830 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: JSR has developed this grade as the only supplier in the world. Applications are broad. For example, the vibration absorbing materials for automobile, films, tubes, rubber shoe soles, some injection molded products and plastic modifiers.

Applications: Various Shoe Soles, Industrial Goods, Melt Bags, Films, Sheets, Hoses, Various Sponge Products, Rubber Modifiers

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/cc
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 99ASTM D2240
Hardness, Shore D 47ASTM D2240
Tensile Strength 12.7 MPaASTM D412
Elongation at Break 670 %ASTM D412
300% Modulus 7.80 MPaASTM D412
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °C
Vicat Softening Point 68.0 °CASTM D1525
Brittleness Temperature -35.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.517ASTM D542
Haze 8.0 %ASTM D1003
Transmission, Visible 82 %ASTM D1003
 
Descriptive Properties
Content (%)93Microstructure, Percentage of 1,2 bonds
Product formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSRC8158 / 295474

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.