MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers TEKAMID® JN920 PPE+PA66 20% Glass Fiber Reinforced PA/PPE Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.

JN-series: PA66/PPE, PA6/PPE alloy (Unreinforced, GF reinforced, MF reinforced)

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 122.6 MPaASTM D638
Elongation at Break 8.0 %ASTM D638
Flexural Strength 194.24 MPaASTM D790
Flexural Modulus 5964 MPaASTM D790
Izod Impact, Notched 8.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 254 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 232 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 305 °C
Mold Temperature 75.0 - 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
Akro-Plastic Akromid® A3 GF 20 black PA 6.6 Dry, 20% Glass Filled
Akro-Plastic Akromid® A3 GF 20 1 black (2307) PA 6.6 Dry, 20% Glass Filled, Heat Stabilized
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Conditioned)
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled

PEPOLZ009 / 103506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.