MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BNZ Materials PA 20 Insulating Firebrick
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirements and after firing is machined to precise tolerances. Made from high purity refractory clays and other ceramic raw materials, these IFB contain a carefully graded organic filler which is burned out during manufacture to give a uniform controlled pore structure.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 39.0 lb/ft³ASTM C134
Deformation 0.50 %
@Temperature 1093 °C,
Time 5400 sec
10 psi load, Hot Load Strength; ASTM C16
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000590 GPa
Compressive Strength 7.00 kg(f)/cm²Cold Crush Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.60 µm/m-°C
@Temperature 20.0 - 1093 °C
Thermal Conductivity 0.200 W/m-K
@Temperature 260 °C
ASTM C182
 0.260 W/m-K
@Temperature 538 °C
ASTM C182
 0.320 W/m-K
@Temperature 816 °C
ASTM C182
 0.350 W/m-K
@Temperature 1093 °C
ASTM C182
Maximum Service Temperature, Air 1093 °C
Shrinkage 0.00 %
@Temperature 1232 °C,
Time 86400 sec
Permanent Linear Change; ASTM C210
 
Component Elements PropertiesOriginal ValueComments
Al2O3 42.5 %
CaO 2.5 %
Fe2O3 0.70 %
MgO 0.10 %
Na2O 1.0 %Includes K2O
SiO2 51.5 %
TiO2 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

CBNZ924 / 149164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.