MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1300 TC-I-20 Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Insulative - Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.90 g/cc2.90 g/ccASTM D 792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 96.5 MPa14000 psiASTM D 638
Elongation at Break <= 1.0 %<= 1.0 %ASTM D 638
Tensile Modulus 15.9 GPa2300 ksiASTM D 638
Flexural Strength 145 MPa21000 psiASTM D 790
Flexural Modulus 15.9 GPa2300 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.20 mm
0.800 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 1.87 J/cm
@Thickness 3.20 mm
3.50 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D 257
Dielectric Constant 10.1
@Frequency 1e+6 Hz
10.1
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.8 µm/m-°C11.0 µin/in-°FASTM E 831
CTE, linear, Transverse to Flow 41.4 µm/m-°C23.0 µin/in-°FASTM E 831
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°FThrough-plane; E 1530
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 307 - 329 °C585 - 625 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
RTP Company RTP 1300 TC-C-30 Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Conductive - Flame Retardant
RTP Company RTP 1399 X 102903 J Polyphenylene Sulfide (PPS) Thermally Conductive - Electrically Insulative
RTP Company RTP 399 X 95997 B Polycarbonate (PC), Thermally Conductive - Electrically Conductive
ALM PA 605-A Filled Nylon 12 Prototyping Polymer

PQZTA21615 / 159138

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.