MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Compounds Armamid® PA6 GF 15-1THSM Nylon 6, 15% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: A 15% glass fiber, heat-stabilized polyamide 6. This material displays high mechanical and electrical properties; resilient to hydrocarbons (kerosene, gasoline, benzene etc.), mineral and synthetic oils, strong and weak alkali, weak acids. Designed for injection molding of items and parts for a wide solutions range: construction, electronics, auto industry, machine engineering, aviation, household, transportation etc. Available in natural, gray and black colors.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 250 °C
15 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 110 MPa16000 psiISO 527-1
Elongation at Break 5.0 %5.0 %ISO 527-1
Flexural Strength 156 MPa22600 psiat maximum load; ISO 178
Flexural Modulus 4.80 GPa696 ksiISO 178
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -40.0 °C
23.8 ft-lb/in²
@Temperature -40.0 °F
ISO 179-1
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1
Charpy Impact, Notched 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Strength 25.0 kV/mm635 kV/inIEC 20243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
Melting Point 218 °C424 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FISO 75
Glow Wire Ignition Temperature 650 °C1200 °FIEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °F
Mold Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC012 / 307084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.