MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Addolink® 1604 Crosslinking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Addolink 1604, an aromatic diamine, is used as a crosslinking agent in combination with prepolymers for the manufacture of high-quality heat curing PUR elastomers, giving considerably longer casting times than other amine crosslinking agents.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.132 g/cc
@Temperature 110 °C
 1.14 g/cc
@Temperature 100 °C
 1.148 g/cc
@Temperature 90.0 °C
Water Absorption <= 0.15 %
Viscosity 12 cP
@Temperature 110 °C
 19 cP
@Temperature 100 °C
 27 cP
@Temperature 90.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 86.0 - 94.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature <=30.0 °C
 
Descriptive Properties
Appearanceyellow or brown granules
Specifications117-124Average equivalent weight (on amine) RC-method A0192:

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8203 / 208596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.