Notes: 60GS7HX is a 35% glass bead reinforced grade of nylon 6 that offers good balance of mechanical performance coupled with and improved dimensional accuracy. This grade is also heat stabilized for good endurance at elevated service temperatures. Availability: Europe Fillers/Reinforcement: Glass Bead, 35% Filler by Weight Additive: Heat Stabilizer Features: Heat Stabilized; Low Shrinkage; Medium Rigidity Processing Method: Injection Molding Information provided by Teknor Apex |