MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI LARPEEK 50 G/20 20% Glass Reinforced Polyetheretherketone (PEEK)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°C), offers outstanding wear performance and has a comprehensive resistance to chemicals and aggressive agents. Larpeek compounds are intrinsically flame retardant and maintain UL94 V0 rating in thin walled products without requiring any special additive. Larpeek compounds can substitute metals, ceramics, and composites in many engineering applications offering improved performance together with simplified production, reduced cost and extended reliability.

Specific Notes for this Material: PEEK, 20% glass fiber, flame retardant UL94 V0, halogens and red phosphorous free

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inLATI
Linear Mold Shrinkage, Transverse 0.0115 cm/cm0.0115 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 140 MPa20300 psiISO 527
Flexural Modulus 7.70 GPa1120 ksiASTM D790
Izod Impact, Notched 0.770 J/cm
@Temperature 23.0 °C
1.44 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 - 390 °C698 - 734 °F
Mold Temperature 180 - 190 °C356 - 374 °F
Drying Temperature 150 - 170 °C302 - 338 °FAlways recommended, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourAlways recommended, drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced
Overview of materials for Polyetheretherketone, Glass Fiber Filled
VICTREX™ PEEK 450GL30 Blk Polyetheretherketone, 30% Glass Fiber, Black
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Solvay APC-2/S-2 Glass PEEK with Glass Fiber Reinforced Unidirectional Tape

PLATI243 / 50241

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.