System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NAECO® ELKON® R20 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12
Categories:
Metal
;
Metal Matrix Composite
;
Nonferrous Metal
;
Refractory Metal
;
Tungsten Alloy
Material Notes:
For projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members.
Formerly CMW® ELKONITE® 30W3
Information provided by NAECO, LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
15.56
g/cc
0.5621
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell B
103
103
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00000421
ohm-cm
0.00000421
ohm-cm
(41% IACS)
Thermal Properties
Metric
English
Comments
Thermal Conductivity
145
W/m-K
1010
BTU-in/hr-ft²-°F
Melting Point
1080
-
3410
°C
1980
-
6170
°F
Solidus
1080
°C
1980
°F
Liquidus
3410
°C
6170
°F
Component Elements Properties
Metric
English
Comments
Copper, Cu
20 %
20 %
Tungsten, W
80 %
80 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NAECO® ELKON® R45 Copper Tungsten RWMA Class 10
NAECO® ELKON® R25 Copper Tungsten RWMA Class 11
NAECO® ELKON® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated
NAECO® ELKON® 2140C Copper Tungsten Nickel material
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
NCMV839 / 192435
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.