Standard Applications: RHODOLINE® 271 is highly efficient anionic dispersant for pigments used in latex paints and adhesives. Recommended usage level is typically 0.2 - 0.5% (dry solids) by weight on pigment, depending upon the system. The optimum level of RHODOLINE® 271 may be determined by the pigment dispersant demand method Chemical Name: ACRYLIC POLYMER Information provided by Solvay |