MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 797915 sec; ASTM D2240
Tensile Strength, Yield 41.4 MPa6000 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.99 GPa434 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 81.2 MPa11800 psiASTM D790
Flexural Modulus 2.91 GPa422 ksiASTM D790
Izod Impact, Notched  10.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
18.7 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
 12.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
22.5 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy  48.9 J/cm
@Temperature 23.0 °C
0.0916 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 173 J/cm
@Temperature 23.0 °C
0.324 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
163 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.899 mm
V-0
@Thickness 0.0354 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
Agency RatingsCSA A440-M90
Ease of SizingExcellent
FeaturesGood Impact Resistance
 Good UV Resistance
 Good Weather Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
PVC Cell Classification1-41434-33ASTM D4216
 16354ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100 BK602 POM
Overview of materials for Acetal Copolymer, Unreinforced
Delrin Delrin® 100 NC010 POM
Geon® Performance Solutions 81530 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid

PH0POL0230 / 144799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.