MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tetrabromosilane, SiBr4
Categories: Fluid

Material Notes: CAS Number: 7789-66-4

Physical Form: Colorless Fuming Liquid

Key Words: SiBr4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
Molecular Weight 347.702 g/mol
 
Chemical PropertiesOriginal ValueComments
Critical Temperature 390 °C
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.000126cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 109.0 J/gAt Boiling Point
Specific Heat Capacity 0.2793 J/g-°CGas
Melting Point 5.20 °C
Boiling Point 154 °C
Heat of Formation -457.3 kJ/molCrystal
 -415.5 kJ/molGas
 
Descriptive Properties
SolubilityReacts with H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSix Capran® NyLid™ WMB 175 Nylon/EVOH Lidding Film
AdvanSix Capran® NyLid™ WMB 250 Nylon/EVOH Lidding Film
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)

EINOR3079 / 5176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.