MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Fibracon® PTFE + 33% Carbon + 2% Graphite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes: Product characteristics:
  • Improved wear resistance
  • Improved thermal and electrical conductivity
  • Reduced deformation under load
Product applications:
  • Commonly used for piston and seal rings in the compressor industry
  • Dry, poorly lubricated environments

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.04 g/ccASTM D4894
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64 - 70Needle
Tensile Strength 12.0 MPaASTM D4894
Elongation at Break 40 %ASTM D4894

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
AGC Fluon® RB2515 15% Carbon Fiber, PTFE Filled Compound
AGC Fluon® PB3360T 60% Bronze, PTFE Filled Compound
AGC Fluon® PB2510 10% Carbon Fiber, PTFE Filled Compound
AGC Fluon® FC160-60 PTFE, 60% Bronze Filled

PROCH9141 / 232844

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.