MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 3 wt% Multi-Wall Carbon Nanotubes
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PC1501 is a conductive masterbatch based on polycarbonate. Because of its low viscosity and high flow formulation, PLASTICYL™ PC1501 is ideal for standard injection molding and extrusion processes.

Key Applications:

  • E&E, automotive and packaging industries
  • HDD (hard disk drive) internal components
  • HDD and IC handling trays

Benefits:

  • Excellent electrical conductivity at low loading
  • Excellent surface cleanliness
  • Retention of key mechanical properties
  • Ease of processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 3 %Carbon Nanotube Loading
Melt Flow 0.90 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133:1997
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16.0 MPaISO 527-1,2
Tensile Modulus 2.683 GPaISO 527-1,2
Charpy Impact, Notched 6.00 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 54 ohm-cm3.0 wt% carbon nanotubes in PC; CTM E043
 100 ohm-cm2.5 wt% carbon nanotubes in PC; CTM E043
 1200 ohm-cm2.0 wt% carbon nanotubes in PC; CTM E043
 30000 ohm-cm1.5 wt% carbon nanotubes in PC; CTM E043
Surface Resistivity per Square 1200 ohm3.0 wt% carbon nanotubes in PC; CTM E042
 4000 ohm2.5 wt% carbon nanotubes in PC; CTM E042
 17000 ohm2.0 wt% carbon nanotubes in PC; CTM E042
 800000 ohm1.5 wt% carbon nanotubes in PC; CTM E042
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 °CMaterial Temperature
Mold Temperature 120 °C
Hold Pressure 45.0 MPa
Back Pressure 4.00 MPa
 
Descriptive Properties
Processing: Holding Time8 s
Processing: Injection Speed30 cm³/s
Processing: Plasticizing Speed0.4 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daicel CEVIAN® CGF20 20% GF PC/Acrylic Alloy
Nanocyl PLASTICYL™ PP2001 Polypropylene with 5 wt% Multi-Wall Carbon Nanotubes
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes
BASF Ultraform® E 3120 BM POM

PNANOCY972 / 108927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.