Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celcon® CF801 Dissipative, General Purpose Material
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Unreinforced
Material Notes:
Description:
Celcon CF801 is a dissipative, general purpose material.
Information provided by Celanese Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.38
g/cc
0.0499
lb/in³
ISO 1183
Linear Mold Shrinkage
0.019
cm/cm
0.019
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.017
cm/cm
0.017
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
50.0
MPa
7250
psi
50 mm/min; ISO 527-2/1A
Tensile Modulus
2.40
GPa
348
ksi
1 mm/min; ISO 527-2/1A
Flexural Modulus
2.30
GPa
334
ksi
ISO 178
Izod Impact, Notched (ISO)
4.20
kJ/m²
2.00
ft-lb/in²
ISO 180/1A
Charpy Impact, Notched
0.450
J/cm²
2.14
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
60000
ohm-cm
60000
ohm-cm
IEC 60093
Surface Resistance
1000
ohm
1000
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
70.0
°C
158
°F
ISO 75-1, -2
Processing Properties
Metric
English
Comments
Melt Temperature
182
-
199
°C
360
-
390
°F
Mold Temperature
77.0
-
93.0
°C
171
-
199
°F
Drying Temperature
82.2
°C
180
°F
Dry Time
3
hour
3
hour
Injection Pressure
75.8
-
110
MPa
11000
-
16000
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celcon® AS450 Acetal Copolymer
Celanese Celcon® C13031 XF Acetal Copolymer
Celanese Celcon® AS270 Acetal Copolymer
Celanese Celcon® LW90-F2 POM, Tribological
BASF Ultraform® H 2320 006 Q600 POM
PHCW24 / 45965
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.